(January 5, 2021 at 10:12 am)Fireball Wrote:(January 5, 2021 at 7:40 am)onlinebiker Wrote: Ok.... I guess you meant MIG, not TIG......You're right-MIG. And it's flux core, which I believe is part of the problem as well.
Now - are you using flux core wire or mixed gas (C25)?
Ok... If your machine has the option for gas feed - upgrade to it.
Flux core is essentially the same as stick welding - with the smoke... Plus you get splatter all over. That contributes to ugly welds. You get cleaner welds and breatheable air using gas feed.
Also - if your machine is gas capable - make sure your polarity is correct.
Flux core = negative to stinger.
Gas feed = negative to workpiece.
That got me once... Couldn't get a good weld at all...